EN

Calculate Concrete and Mortar Mix Ratios

Making good concrete or mortar comes down to precise proportions of cement, sand, gravel and water — the mix ratio depends on the job: foundation concrete, reinforced concrete, tile screed, block-laying mortar… Choose the mix type, enter the volume to pour (from dimensions or directly), and the exact quantities plus the number of cement bags follow.

Concrete and mortar mixed at the same cement content don't have the same strength: the finer the aggregate, the more cement it takes to bind the particles. At an equal mix ratio, concrete — whose gravel supplies most of the strength — is stronger than mortar.

Mix type and volume

Concrete or mortar type
Dimensions of the job
Volume to pour
Margin and container

Increases the quantities to buy, to avoid running short mid-job.

For mixing without a scale: a standard 10 L builder's bucket, or a calibrated shovel.

Trade terms tagged with an asterisk are defined in the glossary at the foot of the page.

Concrete is not mortar

The heap on the drive gets called “cement” more often than it should. Cement is the grey powder in the bag. What comes out of the drum is either concrete or mortar. Both are mixed with water. They do not do the same job, and they do not carry the same stone.

Mortar is cement, sand and water. No coarse aggregate*. It beds a block, points a joint, renders a wall, grouts a fixing. A 10 mm bed has no room for 20 mm stone. Concrete is that same paste plus gravel — 10 mm, 20 mm, sometimes a graded 4/20. The stone is the skeleton. The paste only glues the grains. Without that skeleton, a floor slab is expensive mortar. It cracks. It does not span.

Swap them and the job fails in a morning. “Concrete” in a block joint traps pebbles and leaves voids; the block rocks. Mortar in a strip footing burns bags of cement and still has no backbone. A sand/cement screed is not a slab either: no stone, richer cement, 40 to 75 mm, never 100. After all, the pointing trowel and the mixer shovel belong to different trades.

Lime in the binder is a third mix again. Cement-lime mortar — gauged mortar — is fatter and more plastic than a straight cement mix. It suits brick and stone that need to move a little. For new dense blocks, a cement mortar at about 300 to 350 kg/m³ is the usual bed, and the count of units is a separate job, done with the block and brick quantity calculator.

Matching the mix to the job

The mix ratio is not a matter of taste. Blinding under a footing is not asked to carry a house. A garage slab sees tyres, frost, sometimes de-icing salt. A bag labelled “concrete mix” with no strength class says nothing about any of that.

C25/30* is the site default for anything that carries load: strip foundation, ground beam, garage floor. 25 MPa on a cylinder, 30 on a cube, at 28 days. Below that, C12/15 or the old GEN1, for blinding. Above it, C30/37, the work leaves the bag: a plant mix, often an engineer. BS EN 206*, with BS 8500 in the UK, talks in classes, not in “an extra shovel because it is a garage”.

  • Blinding — 50 mm or so, C12/15, around 150 kg of cement per cubic metre. A clean, level bed under a footing. It does not enter the bearing calculation.
  • Foundations — C25/30 as a rule. On bags, 300 to 350 kg/m³. Clean water, washed aggregate. A house strip footing lives here, provided the ground and the loads have been looked at.
  • Garage or workshop slab — still C25/30, 100 to 150 mm, mesh on spacers. Eighty millimetres “because it is flat” opens on the first frost, or under a van wheel.
  • Reinforced work — the mix does not replace the steel. Chloride-free water, no salt in the sand, proper cover. Bar counts, laps and mesh weight belong to the slab rebar calculator. This page batches the paste that covers them.

A plant C25/30 is not a 1:2:4 bucket mix. The plant weighs, trims the water, delivers a class. A 90-litre drum delivers a batch. On a small pad they can land in the same neighbourhood. On a beam, a column, a suspended floor, the class is ordered. It is not guessed from the colour of the mix.

What cement, sand and stone actually do

Three heaps, plus water. Each has a job.

Cement binds. With water it hydrates, sets, hardens. The common bag is CEM II, or OPC* — CEM I — when a plain Portland is wanted. CEM I is livelier in the cold. A slag cement (CEM III) is slower, cooler, better in large pours. The 32,5 or 42,5 on the bag is the cement's class, not the concrete's. A poorly batched 42,5 still makes weak concrete. A well batched 32,5, kept wet, puts an honest C25/30 on the cube.

Sand, 0/4 mm, fills the voids between the stones. Without it the paste runs and the mix is full of holes. Too much sand and there is not enough coarse stone to carry load — the mix has become mortar, and it drinks extra water to stay workable. Gravel, 10 mm or 20 mm, is the skeleton. 10 mm packs around tight mesh. 20 mm in a 80 mm slab jams.

A working site mix at 250–300 kg of cement per cubic metre sits around 700 kg of sand and 1,100 to 1,200 kg of stone, plus 130 to 170 litres of water. Combined ballast* — sand and gravel already blended — cuts a heap. It does not remove the need to weigh the cement or to measure the water. Too many fines and the batch is thirsty: more water goes in, and the cube strength drops. A mix that stands on the shovel is not the soup that runs through the drum blades.

Water, the w/c ratio and slump

Water is not free lubrication. It hydrates the cement — no water, no set — and it opens pores the moment there is too much of it. The ratio that matters is w/c*: mass of water over mass of cement. Not the hose “until it looks like porridge”.

w/c = mass of water / mass of cement  ·  aim 0.45 to 0.55

Below 0.35 the paste does not hydrate fully and will not compact; honeycombing follows. Past 0.60 the mix places easily, looks fine under the rule — and is porous. Frost, carbonation, rust on the steel. The useful window on a careful job is 0.45 to 0.55. A plasticiser drops w/c at the same slump*. That bottle, not the tap, is how a wetter look is bought without drowning the batch.

Nobody brings an Abrams cone to a garden pour. The shovel is the test. A plastic mix that slumps without collapsing will tamp and rule. Too dry, voids. Too wet, bleed, a dusty surface later. Rain in the sand already counts toward w/c: a heap left uncovered, and the measured bucket is already too much. One litre of water is one kilogram, so 165 L on 300 kg of cement is w/c = 0.55. The cube-killer remains the extra bucket “because it is stiff”. Strength has already dropped 20 to 40 %.

Sharp sand, builders' sand, marine sand

Not every sand belongs in the drum. Grain shape, salt, dirt: three different problems, and dirt is the common one.

Sharp sand — grit, angular — grips. Concrete likes it. Mortar works harder with it. Builders' sand, the soft, rounded stuff, trowels like butter and is lazy in a structural mix. River sand, washed and rounded, is the easy mixer for mortar and screed. Quarry sand, crushed, is harsher and gives a bit more mechanical interlock in concrete.

Marine sand carries chlorides. In reinforced work the salt attacks the steel, cover or no cover. Out of the question on a garage slab. Dune sand sold unwashed is not sharp sand from a pit. At a pinch it goes in unreinforced fill, not around mesh. That said, the sand from the back of the garden is the one that actually turns up: roots, silt, organics. Set is poor, the surface dusts, brown stains show. A handful in a bucket of clean water: if it clouds and will not settle, the heap is dirty. Wash it, or change it. Washed pit sand costs more than the neighbour's pile. Less than a slab that has to come out.

Set, curing, the 28-day cube

Three clocks, one word people mash together: “drying”.

Set is the hour or two when the paste stops being plastic. The trowel no longer leaves a mark. A lively CEM I at 25 °C can pull in a couple of hours. A slag cement at 10 °C takes longer. In that window the mix is compacted, ruled, finished. After it, the cracks are being decorated.

Strength is hydration, not a towel in the sun. Cement wants water for days, not a draught. The slab is kept damp — sprayed, covered, curing compound. It is not “left to dry”. Dry it too soon and the surface stops hydrating, dusts, micro-cracks. At 7 days, around 70 % of the 28-day strength for an ordinary Portland. At 28 days, the class is judged. Gain goes on for months after that, slower, if the first week was kept wet. A C25/30 at 90 days is stronger than at 28 — provided it was not baked on day two.

Striking a column at four because it feels hard is a different trade. Formwork times sit in BS EN 13670, by temperature and thickness. A 120 mm slab at 15 °C is not a driveway the next morning. A week of curing, no frost, no bare midday sun, is not luxury. At 5 °C the pour itself is in question. At 30 °C the mix shortens, the heaps are shaded, water goes on early.

Casting a slab: hardcore, DPM, formwork

The concrete is only the top layer. What holds it is underneath.

Hardcore, 100 to 200 mm of compacted type-1 or similar, in layers, drains and spreads load. Soft, unlevelled ground, and the slab cracks where the soil settles, whatever the mix. Over that, a DPM, laps taped, turned up at the edges. It cuts rising damp and stops laitance vanishing into the stone. Formwork, level, stiff enough not to belly under 2.5 tonnes per cubic metre. A garage slab, 100 mm as a floor, 150 mm if a van parks on it. Eighty millimetres is a screed. It is not a parking bay.

Mesh — A142, A193, according to span and load — sits on spacers, not on the DPM. Mesh on the bottom does no work. Mesh at the surface rusts. Cover of 40 mm or so on an external slab is not an architect's whim. Bar lengths and steel weight are a separate take-off. This page is about the paste. One continuous pour, or wet-to-wet joints. A cold joint across 20 m² is a crack with a date on it. Movement joints every 4 to 6 m, or the slab picks its own line — often a diagonal, often at a doorway. Tamp, rule, trowel, then cure. In short, the calculator counts bags. It does not compact the hardcore.

Worked quantities for a 20 m² garage floor

A 5 × 4 m rectangle, 130 mm thick. The volume is not a riddle.

V = A × t  →  20 × 0.13 = 2.6 m³

A site-style C25/30 at 300 kg of cement per cubic metre: 300 kg cement, 700 kg sand, 1,100 kg of 20 mm, 165 L of water. For 2.6 m³: 780 kg of cement, 1.82 t of sand, 2.86 t of stone, 429 L of water. That is 32 bags of 25 kg, plus about 10 % waste. The form on this page does that sum, margin included. The ready-mix* lorry bills by the cubic metre delivered, often with a 4 or 5 m³ minimum. At 2.6 m³, bags still make sense. Past that, the plant wins. Mesh, DPM and hardcore never appear in the mass table. They still sit in the quote, and in the slab.

A 1:2:4 bucket mix is not a strength class. Columns, beams, suspended floors: an engineer. This page is a batch quantity, not a design note.

A drum mixer is not a batching plant

The 90-litre mixer on the drive is not a plant drum. It stirs. It does not weigh. Usual order: a little water, stone (it scours the drum), sand, cement, the rest of the water. Three minutes, not thirty. Too long and the mix starts to go off in the drum. Too short, pockets of dry cement.

The stamped capacity is not the useful load. A 90-litre machine batches more like 50 to 60 litres of concrete. Buckets are counted on that, not on a drum filled to the rim. Ballast goes in by the shovel, cement by the whole bag if possible, so a bag is not split by eye. A 10-litre bucket, always the same one, beats three different shovels according to who is loading. At 5 °C the pour waits. Frostproofer does not license a pour onto frozen hardcore. At 30 °C the heaps are shaded, the mix is shortened, the pour is early. The plant has a clock and a mix temperature. The drive does not.

Plasticiser, not another gallon

Plasticiser, retarder, accelerator, frostproofer. Four bottles, four jobs. None of them is a substitute for a mix ratio.

A plasticiser cuts w/c at the same slump. The batch holds together without the fatal extra bucket. A retarder stretches the set if the slab is long or the day is hot. An accelerator is a cold-weather tool. Frostproofer lowers the freezing point of the mix water. It does not make concrete set at −5 °C on frozen ground. The data sheet, the cap dose, not a splash by eye. An overdose segregates the mix. The bottle is a plant tool come down to the bag. It is measured. It is not a second hose.

Bags, ballast or the ready-mix lorry

Three roads to the same cubic metre, and they are not equal for consistency.

Bags, 25 kg, plus heaps of aggregate, plus the mixer. Flexible, slow, uneven from batch to batch if the water is guessed. Workable up to 2 or 3 m³. A bulk bag of ballast cuts a heap. Cement and water stay separate. A decent compromise for a patio, a small wall, a modest garage. The lorry delivers a class, w/c under control, slump ordered (S3, S4). For 6 m³ of footing, that is the vehicle. For 600 litres of pads, it is the bag. Even so, a 25 kg “ballast mix” bag is a fixing or a small pad. It does not price a 20 m² slab: the cost per cubic metre takes off, and the class is not always printed.

This page spits masses. The volume plus a 5 to 10 % margin says whether the plant is worth the call.

Lime in the mortar, and pointing

Straight cement mortar at 350 kg/m³ is stiff, tight, brittle. On a new dense block it holds. On old brick or stone it is too strong: the joint becomes harder than the face, and the face fails.

Gauged mortar cuts the cement with lime. Fatter, more flexible, it trowels, it takes a little movement. A common gauge is 1 cement : 1 lime : 6 sand. It is not concrete. No gravel. Joints, render, stone bedding. Pointing is batched a little richer and placed drier, so it does not stain. Bedding mortar is wetter, to grab the block. The form already splits the two. Lime is a binder choice, not a volume the calculator converts.

Glossary

Aggregate
Sand and stone, sized (0/4, 10 mm, 20 mm…). The skeleton of concrete. Mortar has only the sand; concrete adds the coarse fraction.
C25/30
Concrete strength class under EN 206 / BS 8500. Characteristic compressive strength 25 MPa on a cylinder, 30 MPa on a cube, at 28 days. The usual spec for a strip footing or a garage slab.
BS EN 206
The British adoption of the European standard that classifies concrete by strength, consistence and exposure. In the UK it is used with BS 8500, which sets the complementary rules for mix specification.
OPC
Ordinary Portland cement, broadly CEM I in EN 197-1. The “plain” Portland. CEM II is a composite Portland (limestone, slag, fly ash). The 32,5 / 42,5 figure is the cement class, not the concrete class.
Ballast
Sand and gravel already combined, sold loose or in bulk bags, for site concrete. Cement and water are still added separately. Not the same as a complete dry mix in a bag.
w/c
Water/cement ratio by mass. Mix water divided by cement mass. Around 0.45 to 0.55 for a decent structural mix. Higher means more pores and less strength.
Slump
Settlement of fresh concrete in the Abrams cone, in millimetres (classes S1 to S5). High slump without a plasticiser usually means too much water.
Ready-mix
Concrete batched at a plant and delivered in a drum lorry, sold by the cubic metre, to a specified class and slump. Opposite of a site mix from bags.

Related calculators